After patching refractory with plastic firebrick, holes are poked in the patch on 1 1/2 inch centers in order to __________.
- Aprevent spalling
- Bvent escaping moisture ✓
- Callow for expansion
- Dprevent slag buildup
Correct answer: B) vent escaping moisture