In order to prevent galvanic corrosion, an aluminum boat must be insulated from the davits and gripes. Which of the following is acceptable as an insulator?

  1. AHard rubber ✓
  2. BCanvas
  3. CLeather
  4. DSponge rubber

Correct answer: A) Hard rubber