To combat galvanic corrosion, condensers utilizing copper-nickel water boxes are usually fitted with __________.

  1. Abonding straps
  2. Biron or steel anodes
  3. Cprotective coatings
  4. Dall of the above ✓

Correct answer: D) all of the above

USCG question bank (2008) · Steam Plants – Question Bank Book 13 · pass mark 70%